GB/T 14017-2009   Method of testing in tensile strength perpendicular to grain of wood (English Version)
Standard No.: GB/T 14017-2009 Status:superseded remind me the status change

Email:

Target Language:English File Format:PDF
Word Count: 4000 words Translation Price(USD):100.0 remind me the price change

Email:

Implemented on:2009-8-1 Delivery: via email in 1~3 business day

→ → →

,2023-2-1,2009-8-1,141138181865371B2816B4E91ED1C
Standard No.: GB/T 14017-2009
English Name: Method of testing in tensile strength perpendicular to grain of wood
Chinese Name: 木材横纹抗拉强度试验方法
Chinese Classification: B60    Basic standard and general method on forestry
Professional Classification: GB    National Standard
Source Content Issued by: AQSIQ; SAC
Issued on: 2009-02-23
Implemented on: 2009-8-1
Status: superseded
Superseded by:GB/T 1927.15-2022 Test methods for physical and mechanical properties of small clear wood specimens—Part 15: Determination of tensile strength perpendicular to grain
Superseded on:2023-2-1
Superseding:GB/T 14017-1992 Method of testing in tensile strength perpendicular to grain of wood
Target Language: English
File Format: PDF
Word Count: 4000 words
Translation Price(USD): 100.0
Delivery: via email in 1~3 business day
本标准规定了测定木材横纹抗拉强度的试验设备、试样、试验步骤和结果计算等。
本标准适用于木材无疵小试样的横纹抗拉强度试验。
Code of China
Standard
GB/T 14017-2009  Method of testing in tensile strength perpendicular to grain of wood (English Version)
Standard No.GB/T 14017-2009
Statussuperseded
LanguageEnglish
File FormatPDF
Word Count4000 words
Price(USD)100.0
Implemented on2009-8-1
Deliveryvia email in 1~3 business day
Detail of GB/T 14017-2009
Standard No.
GB/T 14017-2009
English Name
Method of testing in tensile strength perpendicular to grain of wood
Chinese Name
木材横纹抗拉强度试验方法
Chinese Classification
B60
Professional Classification
GB
ICS Classification
Issued by
AQSIQ; SAC
Issued on
2009-02-23
Implemented on
2009-8-1
Status
superseded
Superseded by
GB/T 1927.15-2022 Test methods for physical and mechanical properties of small clear wood specimens—Part 15: Determination of tensile strength perpendicular to grain
Superseded on
2023-2-1
Abolished on
Superseding
GB/T 14017-1992 Method of testing in tensile strength perpendicular to grain of wood
Language
English
File Format
PDF
Word Count
4000 words
Price(USD)
100.0
Keywords
GB/T 14017-2009, GB 14017-2009, GBT 14017-2009, GB/T14017-2009, GB/T 14017, GB/T14017, GB14017-2009, GB 14017, GB14017, GBT14017-2009, GBT 14017, GBT14017
Introduction of GB/T 14017-2009
本标准规定了测定木材横纹抗拉强度的试验设备、试样、试验步骤和结果计算等。
本标准适用于木材无疵小试样的横纹抗拉强度试验。
Contents of GB/T 14017-2009
About Us   |    Contact Us   |    Terms of Service   |    Privacy   |    Cancellation & Refund Policy   |    Payment
Tel: +86-10-8572 5655 | Fax: +86-10-8581 9515 | Email: coc@codeofchina.com | QQ: 672269886
Copyright: Beijing COC Tech Co., Ltd. 2008-2040
 
 
Keywords:
GB/T 14017-2009, GB 14017-2009, GBT 14017-2009, GB/T14017-2009, GB/T 14017, GB/T14017, GB14017-2009, GB 14017, GB14017, GBT14017-2009, GBT 14017, GBT14017