2025-12-5 10.1.6.65
Code of China Chinese Classification Professional Classification ICS Classification Latest News Value-added Services

Position: Chinese Standard in English/GB 6458-1986
GB 6458-1986   Metallic coatings—Neutral Salt Spray Tests(NSS tests) (English Version)
Standard No.: GB 6458-1986 Status:superseded remind me the status change

Email:

Target Language:English File Format:PDF
Word Count: 2000 words Translation Price(USD):40.0 remind me the price change

Email:

Implemented on:1980-5-1 Delivery: via email in 1 business day

→ → →

,1998-1-1,1980-5-1,6D0542EEE855FC841430182794694
Standard No.: GB 6458-1986
English Name: Metallic coatings—Neutral Salt Spray Tests(NSS tests)
Chinese Name: 金属覆盖层 中性盐雾试验(NSS试验)
Professional Classification: GB    National Standard
Issued on: 1980-03-18
Implemented on: 1980-5-1
Status: superseded
Superseded by:GB/T 10125-1997 Corrosion tests in artificial atmospheres-Salt spray tests
Superseded on:1998-1-1
Target Language: English
File Format: PDF
Word Count: 2000 words
Translation Price(USD): 40.0
Delivery: via email in 1 business day
1 Test Solution 1.1 Chemically pure sodium chloride is dissolved into distilled or deionized water, to produce a solution at a concentration of 50±5g/L. 1.2 An acidometer is used to measure pH value of the solution, or the precision pH paper calibrated using an acidometer may be used for daily testing. pH value of solution may be adjusted with chemically pure hydrochloric acid or sodium hydroxide. The pH value of salt spray solution collected within the test chamber will be set between 6.5 and 7.2. 1.3 The solution must be filtered prior to use, in order to avoid blocking the nozzle. 2 Test Equipment 2.1 The materials used to manufacture test equipment must be resistant to salt spray corrosion and have no influence on the test results. 2.2 The chamber shall not be less than 0.2 m3 in volume and had better not less than 0.4m3; the liquid drops accumulated on the top shall not fall onto the test specimen. Shape and dimension of the chamber shall be in such that salt spray solution collected within the chamber meets the requirements of 5.2. 2.3 It shall be able to maintain the temperature at each position in the chamber meet the requirements of 5.1. Thermometer and automatic temperature control elements shall be kept at a distance not less than 100mm to the inner wall of the chamber, and it shall be possible to read the results outside the chamber. 2.4 The spray device consists of the following parts.
GB 6458-1986 is referred in:
* JT/T 390-1999 Raised Pavement Markers
*GB/T 13322-1991 Metal coating-Cd-Ti plating of low hydrogan embrittlement
Code of China
Standard
GB 6458-1986  Metallic coatings—Neutral Salt Spray Tests(NSS tests) (English Version)
Standard No.GB 6458-1986
Statussuperseded
LanguageEnglish
File FormatPDF
Word Count2000 words
Price(USD)40.0
Implemented on1980-5-1
Deliveryvia email in 1 business day
Detail of GB 6458-1986
Standard No.
GB 6458-1986
English Name
Metallic coatings—Neutral Salt Spray Tests(NSS tests)
Chinese Name
金属覆盖层 中性盐雾试验(NSS试验)
Chinese Classification
Professional Classification
GB
ICS Classification
Issued by
Issued on
1980-03-18
Implemented on
1980-5-1
Status
superseded
Superseded by
GB/T 10125-1997 Corrosion tests in artificial atmospheres-Salt spray tests
Superseded on
1998-1-1
Abolished on
Superseding
Language
English
File Format
PDF
Word Count
2000 words
Price(USD)
40.0
Keywords
GB 6458-1986, GB/T 6458-1986, GBT 6458-1986, GB6458-1986, GB 6458, GB6458, GB/T6458-1986, GB/T 6458, GB/T6458, GBT6458-1986, GBT 6458, GBT6458
Introduction of GB 6458-1986
1 Test Solution 1.1 Chemically pure sodium chloride is dissolved into distilled or deionized water, to produce a solution at a concentration of 50±5g/L. 1.2 An acidometer is used to measure pH value of the solution, or the precision pH paper calibrated using an acidometer may be used for daily testing. pH value of solution may be adjusted with chemically pure hydrochloric acid or sodium hydroxide. The pH value of salt spray solution collected within the test chamber will be set between 6.5 and 7.2. 1.3 The solution must be filtered prior to use, in order to avoid blocking the nozzle. 2 Test Equipment 2.1 The materials used to manufacture test equipment must be resistant to salt spray corrosion and have no influence on the test results. 2.2 The chamber shall not be less than 0.2 m3 in volume and had better not less than 0.4m3; the liquid drops accumulated on the top shall not fall onto the test specimen. Shape and dimension of the chamber shall be in such that salt spray solution collected within the chamber meets the requirements of 5.2. 2.3 It shall be able to maintain the temperature at each position in the chamber meet the requirements of 5.1. Thermometer and automatic temperature control elements shall be kept at a distance not less than 100mm to the inner wall of the chamber, and it shall be possible to read the results outside the chamber. 2.4 The spray device consists of the following parts.
Contents of GB 6458-1986
About Us   |    Contact Us   |    Terms of Service   |    Privacy   |    Cancellation & Refund Policy   |    Payment
Tel: +86-10-8572 5655 | Fax: +86-10-8581 9515 | Email: coc@codeofchina.com | QQ: 672269886
Copyright: Beijing COC Tech Co., Ltd. 2008-2040
 
 
Keywords:
GB 6458-1986, GB/T 6458-1986, GBT 6458-1986, GB6458-1986, GB 6458, GB6458, GB/T6458-1986, GB/T 6458, GB/T6458, GBT6458-1986, GBT 6458, GBT6458